Common separation processes for copper-lead bulk concentrates include the following:
I. Dichromate Method
This method utilizes dichromate to depress galena, thereby allowing for the flotation and recovery of copper minerals.
II. Cyanide Method
This method employs cyanide to depress copper minerals, enabling the flotation and recovery of lead minerals.
III. Ferricyanide/Ferrocyanide Method
When secondary copper minerals constitute a significant portion of the ore, the two aforementioned methods have limited applicability. If the ore has a relatively high lead content, ferricyanide or ferrocyanide (such as potassium ferrocyanide or potassium ferricyanide) can be used to depress secondary copper minerals, allowing for the flotation and recovery of lead minerals.
In cases where the lead content in the ore is significantly higher than the copper content, the following two process schemes may be tested:
IV. Sulfite (Sulfur Dioxide) Method
Sulfur dioxide gas or sulfite is used to treat the bulk concentrate, which depresses lead minerals while simultaneously activating copper minerals. To enhance the depression effect, reagents such as potassium dichromate or zinc dithionite may be added; alternatively, the pulp can be heated (a "heated flotation" process). At the end of the operation, lime is used to adjust the pulp pH to a range of 5–7 before proceeding with the flotation of copper minerals.
V. Sodium Sulfite–Ferric Sulfate Method
This approach uses a combination of sodium sulfite and ferric sulfate as a depressant, with sulfuric acid added to acidify the pulp. The pulp is stirred at a pH of 6–7 to depress galena, facilitating the flotation and recovery of copper minerals.